Hi Steelers,

I've often been asked how to keep the metal parts on the steel guitar looking like glass. Well, here is a proven way! Some guy's use chrome polish, but the problem with this is that it will leave small scratchs called swirls and it leaves the metal looking frosty.

I use two products and they both work great! The first one is Tecnique Finishing Glaze made by Napa. Here is a link for it.

http://www.martinsenour-autopaint.com/ap/technique_finishing_glaze.htm

The other is 3M Perfect-It 3000 Swirl Mark Remover here is a link where you can get it. http://www.jamestowndistributors.com/userportal/show_product.do?pid=6588&PTECH

I'm not selling or pushing any company, but both of these products work great.. Use this like any other rubbing compound working in small areas until your done. You can go over and over the parts until you get the desired glass finish you want!

I promise you will be blown away by the results. It's great for removing the marks on the fretboard as well. When your done use a good quality wax and your in busniess!

I hope this helps you keep your guitar metal parts looking like glass... It sure works for me!

Thanks,

David C Neal
View user's profile Send private message Send e-mail Visit poster's website
James Morehead


From:
Prague, Oklahoma, USA - R.I.P.
Post  Posted 25 Aug 2007 5:46 am    
Reply with quote

Neat tip there, David! Cool Cool
View user's profile Send private message Send e-mail
Jay Ganz


From:
Out Behind The Barn
Post  Posted 25 Aug 2007 6:26 am    
Reply with quote

I have 3M Finishing Glaze in my Garage. I'm not sure if it will do the same job as the swirl remover though.
View user's profile Send private message Send e-mail Visit poster's website
Erv Niehaus


From:
Litchfield, MN, USA
Post  Posted 25 Aug 2007 6:40 am    
Reply with quote

I have never known "Mother's Mag & Aluminum Polish" to leave swirl marks.
View user's profile Send private message Send e-mail
James Morehead


From:
Prague, Oklahoma, USA - R.I.P.
Post  Posted 25 Aug 2007 7:04 am    
Reply with quote

I use Mother's, and I do'nt think it leaves swirls, either. But it's nice to know what else works well.
View user's profile Send private message Send e-mail
David C Neal


From:
Nashville, TN
Post  Posted 25 Aug 2007 10:48 am     Wax
Reply with quote

I've had some guy's ask me what wax to use.

I use Meguiars NXT Generation Tech Wax Ultimate Deep Gloss.. You can get it at Auto Zone. Its really seems to work best and its great for wood or mica. However if your going to wax wood don't let it dry completely because it will dry in the grain of the wood making it harder to remove and buff to a shine!

Dave
View user's profile Send private message Send e-mail Visit poster's website
Jack Stoner


From:
Kansas City, MO
Post  Posted 25 Aug 2007 11:56 am    
Reply with quote

I'm using a Teflon based auto polish on my mica finished Franklin. It won't hurt the "Franklin" decal on the front either. Also, no fingermarks if you touch the polished aluminum. The name on the polish is "Las Vegas Show Car", but I've seen the same stuff under various names at Fea Markets.

But, if I need to polish any of the polished aluminum, I'll either use Mother's Mag and Aluminum Wheel polish (which is non abrasive) or if I need more I'll start with either Simichrome or MAAS (same stuff)first, which is slightly abrasive, and then the Mother's and finally the Auto polish for the final coat.
View user's profile Send private message Send e-mail
Ken Metcalf


From:
San Antonio Texas USA
Post  Posted 26 Aug 2007 9:49 am     Question
Reply with quote

Shocked Hello Dave,
Does the wax also protect the Alumanannon annon oximydation Laughing
I have found that after getting it shiny it doesn't take much to keep it nice..
How ever my ZB is Really Really bad with little dings
and super dull.. I got a wheel for my drill and buff compound but it seems to work better by hand...
At least thats what she said...
Buffing compound comes in different grits... Just like sand paper..

Kenny
_________________
MSA 12 String E9th/B6th Universal.
Little Walter PF-89.
Bunch of stomp boxes
View user's profile Send private message Send e-mail
Tom Campbell

 

From:
Houston, Texas, USA
Post  Posted 26 Aug 2007 1:34 pm    
Reply with quote

I've used "Mothers" and "Simichrome" and have experienced a foggy end results with both. But, using the 3M Perfect-It gave me the final look I was looking for.
I also frequent a web-site for people that refinish and restore standard guitars. They use nitrocelluous lacquer for refinishing and use the 3M product for the final polishing...(most do this final step by hand).
View user's profile Send private message Send e-mail
David C Neal


From:
Nashville, TN
Post  Posted 26 Aug 2007 8:35 pm     Reply
Reply with quote

Hi Ken,

If your guitar is really bad you might want to have you end plates polished at a shop most shops can do them on the guitar there is a Teflon tape that you can apply to cover the Mica or wood to protect the finish. It’s the same tape they use to apply to the necks of a guitar when you file the frets. Then keep the metal polished by hand with the product of your choice!

Dave
View user's profile Send private message Send e-mail Visit poster's website
Brad Issendorf

 

From:
Lake City, Minnesota
Post  Posted 26 Aug 2007 10:07 pm    
Reply with quote

I also use Mother's on the polished aluminum parts on my MSAs but for a final step, I use some white flour. Just a little bit seems to give it a finer finish than the Mother's alone. It also seems to help the rag pick up more of the left behind polish and oxidation to give it a clearer shine than without.
View user's profile Send private message Send e-mail
Mark Treepaz


From:
Hamburg, New York USA
Post  Posted 27 Aug 2007 6:03 am    
Reply with quote

Brad Issendorf wrote:
I also use Mother's on the polished aluminum parts on my MSAs but for a final step, I use some white flour. Just a little bit seems to give it a finer finish than the Mother's alone. It also seems to help the rag pick up more of the left behind polish and oxidation to give it a clearer shine than without.


White flour??
_________________
Sho-Bud LDG, Gretsch Syncromatic Lap Steel, Fender Steel King amp, Bach Stradivarious 37 Trumpet, Getzen Eterna Flugelhorn, 68 Fender Precision Bass
View user's profile Send private message Send e-mail Visit poster's website
Gil Berry

 

From:
Westminster, CA, USA
Post  Posted 27 Aug 2007 12:40 pm    
Reply with quote

Brad...is that Martha White? lol
View user's profile Send private message Send e-mail
Brad Issendorf

 

From:
Lake City, Minnesota
Post  Posted 27 Aug 2007 3:32 pm    
Reply with quote

No, actually, I'm no cook but I learned this trick when I used to work for a local trucking company as a Diesel mechanic. The drivers in the bulk flour division used to keep even the company tractors polished to the nines. From aluminum fuel tanks to rims. The one thing that they all used after machine buffing was flour, which was readily available because they hauled tons of it everday. There are several different types of flour used to make different products, (ei: coarse ground fine ground, bleached, etc...) but the common everyday, found in the canister at home type was what they used. Other types may work as well, I don't know, but I do know that that was what they used.
View user's profile Send private message Send e-mail
Paul Redmond

 

From:
Illinois, USA
Post  Posted 30 Aug 2007 2:02 am    
Reply with quote

Simichrome applied with a dry cotton ball is tops, but use the stuff sparingly. Keep cleaning off the slurry with fresh, clean cotton balls until it's all gone. It also leaves an oxidation-inhibitor coating on the aluminum to retard the onset of future dulling. It's usually sold by bicycle shops and especially motorcycle shops for keepin' them Harley's lookin' good. If you can't find it there, contact Contenti, Inc. in Providence RI and order direct by credit card from their website. A second choice would be a mix of WD-40 and plain old ordinary talcum powder again used sparingly. Clean off the slurry with rubbing alcohol and cotton balls, then dry ones to finish the job. Used to use this combination to touch up optic finishes in injection mold cavities. BTW for copper and brass, Simichrome cannot be topped.
PRR
View user's profile Send private message Send e-mail
Jack Stoner


From:
Kansas City, MO
Post  Posted 30 Aug 2007 2:29 am    
Reply with quote

If you can't find Simichrome, "MAAS" is sold by many stores (I found it at Walgreen's). It appears to be identical to Simichrome - it's the same color, same consistancy, same slightly abrasive, works identical to Simichrome, and made in Germany the same as Simichrome.
View user's profile Send private message Send e-mail
Danny Hullihen


From:
Harrison, Michigan
Post  Posted 31 Aug 2007 5:43 am    
Reply with quote

Try some of this. No matter how oxidized your aluminum is, it will look like new again. The Mica polish is great too, and it's safe to use on natural body guitars as well.
http://www.jagwirestrings.biz/catalog/c25_p1.html
View user's profile Send private message Send e-mail Visit poster's website

All times are GMT - 8 Hours
Jump to:  
Please review our Forum Rules and Policies
Our Online Catalog
Strings, CDs, instruction, and steel guitar accessories
www.SteelGuitarShopper.com

The Steel Guitar Forum
148 S. Cloverdale Blvd.
Cloverdale, CA 95425 USA

Click Here to Send a Donation

Email SteelGuitarForum@gmail.com for technical support.


BIAB Styles
Ray Price Shuffles for Band-in-a-Box
by Jim Baron